Thermodynamic study of single crystal, Ni-based superalloys in the γ+γ’ two-phase region using Knudsen effusion mass spectrometry, DSC and SEM

Dimitra Spathara, Dmitry Sergeev, Dietmar Kobertz, Michael Michael Müller, Duncan Putman, Nils Warnken