Keyphrases
Differential Scanning Calorimetry
100%
Thermodynamic Study
100%
Single Crystal Ni-based Superalloy
100%
Two-phase Region
100%
Knudsen Effusion Mass Spectrometry
100%
High Temperature
33%
Single Crystal
33%
Temperature Range
33%
Thermodynamic Stability
33%
Thermodynamic Properties
33%
Four Species
33%
Calorimetry Measurement
33%
Electron Energy
33%
Spectroscopic Measurement
33%
Energy Dispersive X-ray Spectroscopy
33%
Ni-based Superalloy
33%
CoCr
33%
Backscattered Electron Imaging
33%
Alnico
33%
Solvus
33%
NiCrBSi
33%
Phase Transition Temperature
33%
Third Generation
33%
CMSX-4
33%
Microstructural Instability
33%
Liquidus Temperature
33%
Incipient Melting
33%
Uprating
33%
Solidus
33%
Vapor Composition
33%
Complex multi-component Systems
33%
Chemistry
Single Crystalline Solid
100%
Differential Scanning Calorimetry
100%
Scanning Electron Microscopy
100%
Mass Spectrometry
100%
Nickel-Based Superalloys
100%
Melting Point
33%
stability
33%
Energy-Dispersive Spectroscopy
33%
Phase Transition Temperature
33%
Physics
Single Crystal
100%
Differential Scanning Calorimetry
100%
Scanning Electron Microscopy
100%
Mass Spectroscopy
100%
Heat Resistant Alloys
100%
Melting Point
33%
Material Science
Differential Scanning Calorimetry
100%
Scanning Electron Microscopy
100%
Ni-based Single Crystal Superalloy
100%
Single Crystal
50%
Nickel-Based Superalloys
50%
Engineering
Two-Phase Region
100%
Melting Point
50%
Phase Transition Temperature
50%
Temperature Range
50%
Liquidus Temperature
50%
Key Importance
50%
Multicomponent System
50%