Original language | English |
---|---|
Publication status | Published - 1 Jan 2005 |
Event | ICC 2005 - Seoul, Korea Duration: 1 Jan 2005 → … |
Conference
Conference | ICC 2005 |
---|---|
City | Seoul, Korea |
Period | 1/01/05 → … |
Yudie Yuan, Rajan Ambat, Brian Connolly, Martin Strangwood, G Scamans, A Afseth, Alison Davenport
Research output: Contribution to conference (unpublished) › Paper
Original language | English |
---|---|
Publication status | Published - 1 Jan 2005 |
Event | ICC 2005 - Seoul, Korea Duration: 1 Jan 2005 → … |
Conference | ICC 2005 |
---|---|
City | Seoul, Korea |
Period | 1/01/05 → … |