Driven by a requirement for increased performance and cost-effectiveness the basic pearlitic microstructures of rail steels are being progressively refined and novel microstructures are being developed With such pi ogress increased attention must be paid to potential weak spots in the microstructure such as non-metallic inclusions For the past few decades rail steels have become progressively cleaner with regard to harmful brittle inclusions however the effect of rolling-sliding contact forces on nominally benign ductile inclusions requires further consideration This work examines the characteristics of ductile Mn-based inclusions in used rail and rail test discs Where the structure near-surface has been subject to a high component of transverse creepage ductile axially aligned inclusion stringers become strain-flattened to form planes of weakness along which micro-cracks initiate and propagate thus facilitating wear and rolling contact fatigue (RCF) cracking The progression of shape change of these ductile inclusions approaching the contact surface has been examined by optical and electron microscopy including focussed ion beam (FIB) analysis As-manufactured ductile inclusions shapes and distributions have also been surveyed with respect to the (geographical) source of the rail steel Comparative data for these different steel sources are given (C) 2010 Elsevier B V All rights reserved
Original languageEnglish
Pages (from-to)733-746
Number of pages14
JournalWear
Volume269
Issue number11-12
DOIs
Publication statusPublished - 1 Oct 2010

Keywords

  • Rail-wheel tribology
  • Rolling contact fatigue
  • Steel
  • MnS based inclusions