Ultra-high temperature deformation in a single crystal superalloy: Mesoscale process simulation and micromechanisms

Research output: Contribution to journalArticlepeer-review

Standard

Ultra-high temperature deformation in a single crystal superalloy : Mesoscale process simulation and micromechanisms. / Tang, Yuanbo T.; D’Souza, Neil; Roebuck, Bryan; Karamched, Phani; Panwisawas, Chinnapat; Collins, David M.

In: Acta Materialia, Vol. 203, 116468, 15.01.2021.

Research output: Contribution to journalArticlepeer-review

Harvard

APA

Vancouver

Author

Tang, Yuanbo T. ; D’Souza, Neil ; Roebuck, Bryan ; Karamched, Phani ; Panwisawas, Chinnapat ; Collins, David M. / Ultra-high temperature deformation in a single crystal superalloy : Mesoscale process simulation and micromechanisms. In: Acta Materialia. 2021 ; Vol. 203.

Bibtex

@article{3d19965f9fdd447e87dbc5b1a9127f64,
title = "Ultra-high temperature deformation in a single crystal superalloy: Mesoscale process simulation and micromechanisms",
abstract = "A mesoscale study of a single crystal nickel-base superalloy subjected to an industrially relevant process simulation has revealed the complex interplay between microstructural development and the micromechanical behaviour. As sample gauge volumes were smaller than the length scale of the highly cored structure of the parent material from which they were produced, their subtle composition differences gave rise to differing work hardening rates, influenced by varying secondary dendrite arm spacings, γ ′ phase solvus temperatures and a topologically inverted γ/γ ′ microstructure. The γ ′ precipitates possessed a characteristic butterfly morphology, resulting from the simultaneously active solute transport mechanisms of thermally favoured octodendritic growth and N-type rafting, indicating creep-type mechanisms were prevalent. High resolution-electron backscatter diffraction (HR-EBSD) characterisation reveals deformation patterning that follows the γ/γ ′ microstructure, with high geometrically necessary dislocation density fields localised to the γ/γ ′ interfaces; Orowan looping is evidently the mechanism that mediated plasticity. Examination of the residual elastic stresses indicated the butterfly γ ′ precipitate morphology had significantly enhanced the deformation heterogeneity, resulting in stress states within the γ channels that favour slip, and that encourage further growth of γ ′ precipitate protrusions. The combination of such localised plasticity and residual stresses are considered to be critical in the formation of the recrystallisation defect in subsequent post-casting homogenisation heat treatments. ",
keywords = "ETMT, HR-EBSD, Micromechanics, Process simulation, Recrysallization, Single crystal, Ultra-high temperature deformation",
author = "Tang, {Yuanbo T.} and Neil D{\textquoteright}Souza and Bryan Roebuck and Phani Karamched and Chinnapat Panwisawas and Collins, {David M.}",
note = "Funding Information: The authors would like to acknowledge the provision of material from Rolls-Royce . D.C. acknowledges financial support from his Birmingham Fellowship and C.P. & Y.T. would like to acknowledge the funding from the Engineering and Physical Science Research Council (EPSRC) under UKRI Innovation Fellowship EP/S000828/1 . Publisher Copyright: {\textcopyright} 2020 Copyright: Copyright 2020 Elsevier B.V., All rights reserved.",
year = "2021",
month = jan,
day = "15",
doi = "10.1016/j.actamat.2020.11.010",
language = "English",
volume = "203",
journal = "Acta Materialia",
issn = "1359-6454",
publisher = "Elsevier",

}

RIS

TY - JOUR

T1 - Ultra-high temperature deformation in a single crystal superalloy

T2 - Mesoscale process simulation and micromechanisms

AU - Tang, Yuanbo T.

AU - D’Souza, Neil

AU - Roebuck, Bryan

AU - Karamched, Phani

AU - Panwisawas, Chinnapat

AU - Collins, David M.

N1 - Funding Information: The authors would like to acknowledge the provision of material from Rolls-Royce . D.C. acknowledges financial support from his Birmingham Fellowship and C.P. & Y.T. would like to acknowledge the funding from the Engineering and Physical Science Research Council (EPSRC) under UKRI Innovation Fellowship EP/S000828/1 . Publisher Copyright: © 2020 Copyright: Copyright 2020 Elsevier B.V., All rights reserved.

PY - 2021/1/15

Y1 - 2021/1/15

N2 - A mesoscale study of a single crystal nickel-base superalloy subjected to an industrially relevant process simulation has revealed the complex interplay between microstructural development and the micromechanical behaviour. As sample gauge volumes were smaller than the length scale of the highly cored structure of the parent material from which they were produced, their subtle composition differences gave rise to differing work hardening rates, influenced by varying secondary dendrite arm spacings, γ ′ phase solvus temperatures and a topologically inverted γ/γ ′ microstructure. The γ ′ precipitates possessed a characteristic butterfly morphology, resulting from the simultaneously active solute transport mechanisms of thermally favoured octodendritic growth and N-type rafting, indicating creep-type mechanisms were prevalent. High resolution-electron backscatter diffraction (HR-EBSD) characterisation reveals deformation patterning that follows the γ/γ ′ microstructure, with high geometrically necessary dislocation density fields localised to the γ/γ ′ interfaces; Orowan looping is evidently the mechanism that mediated plasticity. Examination of the residual elastic stresses indicated the butterfly γ ′ precipitate morphology had significantly enhanced the deformation heterogeneity, resulting in stress states within the γ channels that favour slip, and that encourage further growth of γ ′ precipitate protrusions. The combination of such localised plasticity and residual stresses are considered to be critical in the formation of the recrystallisation defect in subsequent post-casting homogenisation heat treatments.

AB - A mesoscale study of a single crystal nickel-base superalloy subjected to an industrially relevant process simulation has revealed the complex interplay between microstructural development and the micromechanical behaviour. As sample gauge volumes were smaller than the length scale of the highly cored structure of the parent material from which they were produced, their subtle composition differences gave rise to differing work hardening rates, influenced by varying secondary dendrite arm spacings, γ ′ phase solvus temperatures and a topologically inverted γ/γ ′ microstructure. The γ ′ precipitates possessed a characteristic butterfly morphology, resulting from the simultaneously active solute transport mechanisms of thermally favoured octodendritic growth and N-type rafting, indicating creep-type mechanisms were prevalent. High resolution-electron backscatter diffraction (HR-EBSD) characterisation reveals deformation patterning that follows the γ/γ ′ microstructure, with high geometrically necessary dislocation density fields localised to the γ/γ ′ interfaces; Orowan looping is evidently the mechanism that mediated plasticity. Examination of the residual elastic stresses indicated the butterfly γ ′ precipitate morphology had significantly enhanced the deformation heterogeneity, resulting in stress states within the γ channels that favour slip, and that encourage further growth of γ ′ precipitate protrusions. The combination of such localised plasticity and residual stresses are considered to be critical in the formation of the recrystallisation defect in subsequent post-casting homogenisation heat treatments.

KW - ETMT

KW - HR-EBSD

KW - Micromechanics

KW - Process simulation

KW - Recrysallization

KW - Single crystal

KW - Ultra-high temperature deformation

UR - http://www.scopus.com/inward/record.url?scp=85096179174&partnerID=8YFLogxK

U2 - 10.1016/j.actamat.2020.11.010

DO - 10.1016/j.actamat.2020.11.010

M3 - Article

VL - 203

JO - Acta Materialia

JF - Acta Materialia

SN - 1359-6454

M1 - 116468

ER -