The effect of nitrate on salt layers in pitting corrosion of 304L stainless steel

Research output: Contribution to journalArticlepeer-review

Research Projects

  1. Microfocus Synchrotron X-Ray Studies of Localised Corrosion

    Trevor Rayment & Alison Davenport

    ENGINEERING & PHYSICAL SCIENCE RESEARCH COUNCIL

    5/09/074/09/11

    Project: Research Councils