Original language | English |
---|---|
Pages (from-to) | 1610-1611 |
Number of pages | 2 |
Journal | Materials Science and Technology |
Volume | 27 |
Issue number | 10 |
DOIs | |
Publication status | Published - 1 Oct 2011 |
Comments regarding the papers 'On preventing HAZ cracking in laser welded DS Rene 80 superalloy' by Osoba et al. and 'The hot ductility of Nb/V containing high Al, TWIP steels' by Kang et al.
John Campbell
Research output: Contribution to journal › Article
2
Citations
(Scopus)