An innovative method to perform maskless plain waterjet milling for pocket generation: a case study in Ti-based superalloys
Research output: Contribution to journal › Article › peer-review
Authors
Colleges, School and Institutes
Details
Original language | English |
---|---|
Pages (from-to) | 642-648 |
Journal | International Journal of Machine Tools and Manufacture |
Volume | 51 |
Issue number | 7-8 |
Publication status | Published - 1 Jul 2011 |