TY - JOUR
T1 - An experimental investigation into the stress and strain development of a Ni-base single crystal superalloy during cooling from solidification
AU - Qiu, Chunlei
AU - D'Souza, Neil
AU - Kelleher, Joe
AU - Panwisawas, Chinnapat
PY - 2017/1/15
Y1 - 2017/1/15
N2 - In-situ neutron diffraction has been used to study the stress and strain development in a single crystal Ni-base superalloy (CMSX4) during stress relaxation testing under displacement control mode. It was found that the macroscopic strain is dependent not only on stress and temperature but also on time, suggesting that the overall strain development during stress relaxation is a typical visco-plastic behaviour. The visco-plastic and lattice relaxation strain rates were obtained as best-fit equations from the experimentally measured data encompassing a range of stresses and temperatures. The relaxation lattice strain rate was found to be highly dependent on stress and temperature. It was an order of magnitude smaller than the visco-plastic strain in displacement control mode. An in-situ cooling experiment was also carried out but under strain control mode to simulate the casting condition where the metal solidifies and cools in a rigid ceramic mould. It was found that the stress relaxation was significant in this case and the lattice relaxation dominated visco-plasticity in the early stage of cooling. These results were compared with the calculations using the currently developed visco-plastic law and some key points are discussed.
AB - In-situ neutron diffraction has been used to study the stress and strain development in a single crystal Ni-base superalloy (CMSX4) during stress relaxation testing under displacement control mode. It was found that the macroscopic strain is dependent not only on stress and temperature but also on time, suggesting that the overall strain development during stress relaxation is a typical visco-plastic behaviour. The visco-plastic and lattice relaxation strain rates were obtained as best-fit equations from the experimentally measured data encompassing a range of stresses and temperatures. The relaxation lattice strain rate was found to be highly dependent on stress and temperature. It was an order of magnitude smaller than the visco-plastic strain in displacement control mode. An in-situ cooling experiment was also carried out but under strain control mode to simulate the casting condition where the metal solidifies and cools in a rigid ceramic mould. It was found that the stress relaxation was significant in this case and the lattice relaxation dominated visco-plasticity in the early stage of cooling. These results were compared with the calculations using the currently developed visco-plastic law and some key points are discussed.
U2 - 10.1016/j.matdes.2016.10.072
DO - 10.1016/j.matdes.2016.10.072
M3 - Article
SN - 0264-1275
VL - 114
SP - 475
EP - 483
JO - Materials and Design
JF - Materials and Design
ER -