An analytical method to extract irradiation hardening from nanoindentation hardness-depth curves

Research output: Contribution to journalArticlepeer-review

Authors

  • A. Kareer
  • A. Prasitthipayong
  • D. Krumwiede
  • P. Hosemann
  • S. G. Roberts

Colleges, School and Institutes

External organisations

  • University of Oxford
  • UC Berkeley

Abstract

Highlights

A simple nanoindentation post-processing tool is proposed to extract irradiation hardening as a function of dose.

The model separates plasticity size effects, the effect of the underlying unirradiated material and utilises the varying irradiation dose profile.

The model can successfully determines the dose dependent hardness from nanoindentation in heavy-ion irradiated Fe-alloys.

Details

Original languageEnglish
Pages (from-to)274-281
Number of pages8
JournalJournal of Nuclear Materials
Volume498
Publication statusPublished - 1 Jan 2018

Keywords

  • Fe alloys, Ion-irradiation, Irradiation hardening, Nano-indentation