Skip to main navigation Skip to search Skip to main content

Twist drilling of Haynes 282 superalloy

Research output: Contribution to conference (unpublished)Paper

Original languageEnglish
Publication statusPublished - 1 Jan 2011
Event1st CIRP Conference on Surface Integrity (CSI), Jan 30-Feb 01, 2012. Bremen, Germany -
Duration: 1 Jan 2011 → …

Conference

Conference1st CIRP Conference on Surface Integrity (CSI), Jan 30-Feb 01, 2012. Bremen, Germany
Period1/01/11 → …

Keywords

  • Nickel alloy
  • Surface integrity
  • Drilling
  • Twist drilling of Haynes 282 superalloy

    Hood, R., Soo, S., Aspinwall, D., Andrews, P. & Sage, C., 1 Jan 2011, In: Procedia Engineering. 19, p. 150-155 6 p.

    Research output: Contribution to journalArticlepeer-review

    Open Access
    File
    13 Citations (Scopus)
    522 Downloads (Pure)