Studies on the solidification path of single crystal superalloys
Nils Warnken
Metallurgy and Materials
Research output
:
Contribution to journal
›
Article
›
peer-review
12
Citations (Scopus)
402
Downloads (Pure)
Overview
Fingerprint
Fingerprint
Dive into the research topics of 'Studies on the solidification path of single crystal superalloys'. Together they form a unique fingerprint.
Sort by
Weight
Alphabetically
Keyphrases
Solidification Path
100%
Single Crystal Superalloy
100%
High Temperature
33%
After High Temperature
33%
Interdendritic Region
33%
Phase Formation
33%
Superalloy
33%
Microsegregation
33%
Directional Solidification
33%
Extended Exposure
33%
Bridgman Method
33%
Engineering
Single Crystal Superalloys
100%
Great Importance
50%
Eutectics
50%
Microsegregation
50%
Phase Formation
50%
Turbine
50%
Material Science
Single Crystal
100%
Solidification
100%
Superalloys
100%