Original language | English |
---|---|
Pages (from-to) | 109-116 |
Number of pages | 8 |
Journal | Industrial Diamond Review |
Volume | 62 |
Issue number | 593 |
Publication status | Published - 1 Jan 2002 |
Point grinding of nickel-based superalloys
Sein Soo, E-G Ng, Richard Dewes, David Aspinwall, Justin Burrows