Projects per year
Abstract
X-ray computed tomography (XCT) was used to nondestructively observe the hidden corrosion damage operando on aluminum alloy (AA) 7050-T7451 coupled to stainless steel (SS) 304 under a droplet of chloride-containing electrolyte. XCT enabled a three-dimensional assessment of corrosion damage evolution. AA7050 cylinders containing concentric embedded SS304 cylinders simulating a fastener were exposed under NaCl droplets at 97% RH for various times. Both the volume of corrosion damage and the initial volume of constituent particles were monitored and considered for further analysis. Three-dimensional image reconstruction indicated that the combination of stainless steel and constituent particles could support the growth of several corrosion fissures over the exposure period.
| Original language | English |
|---|---|
| Pages (from-to) | 1171-1176 |
| Number of pages | 6 |
| Journal | Corrosion |
| Volume | 71 |
| Issue number | 10 |
| DOIs | |
| Publication status | Published - 1 Oct 2015 |
Keywords
- Aluminum alloy 7050
- Galvanic corrosion
- Simulated fastener
- X-ray computed tomography
ASJC Scopus subject areas
- General Materials Science
- General Chemical Engineering
- General Chemistry
Fingerprint
Dive into the research topics of 'Operando observation of galvanic corrosion between aluminum alloy 7050-T7451 and 304 stainless steel in a simulated fastener arrangement using x-ray tomography'. Together they form a unique fingerprint.Projects
- 1 Finished
-
Microfocus Synchrotron X-Ray Studies of Localised Corrosion
Rayment, T. (Principal Investigator) & Davenport, A. (Co-Investigator)
Engineering & Physical Science Research Council
5/09/07 → 4/09/11
Project: Research Councils