Laser powder bed fabrication of nickel-base superalloys: Influence of parameters; characterisation, quantification and mitigation of cracking

Luke N. Carter, Moataz M. Attallah*, Roger C. Reed

*Corresponding author for this work

Research output: Chapter in Book/Report/Conference proceedingConference contribution

76 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Laser powder bed fabrication of nickel-base superalloys: Influence of parameters; characterisation, quantification and mitigation of cracking'. Together they form a unique fingerprint.

Engineering & Materials Science

Chemistry