Influence of Al and Nb on castability of a Ni-base superalloy, IN713LC

Research output: Contribution to conference (unpublished)Paper

7 Citations (Scopus)
Original languageEnglish
Pages62-65
Number of pages4
DOIs
Publication statusPublished - 1 Aug 2009
Event2nd International Conference on Advances in Solidification Proces, Jun 17-20, 2008. Graz, Austria -
Duration: 1 Aug 2009 → …

Conference

Conference2nd International Conference on Advances in Solidification Proces, Jun 17-20, 2008. Graz, Austria
Period1/08/09 → …

Keywords

  • Fraction liquid
  • Inter-dendritic
  • Ni-alloys
  • Pressure drop
  • Shrinkage porosity