Projects per year
Original language | English |
---|---|
Pages | 66-69 |
Number of pages | 4 |
DOIs | |
Publication status | Published - 1 Aug 2009 |
Event | 2nd International Conference on Advances in Solidification Proces, Jun 17-20, 2008. Graz, Austria - Duration: 1 Aug 2009 → … |
Conference
Conference | 2nd International Conference on Advances in Solidification Proces, Jun 17-20, 2008. Graz, Austria |
---|---|
Period | 1/08/09 → … |
Keywords
- Undercooling
- Misorientation
- Convergence boundary
- Directional Solidification
Projects
- 1 Finished
-
EPSRC/ Rolls Royce Star Appointment in Casting Technology
Engineering & Physical Science Research Council
1/05/05 → 30/04/10
Project: Research Councils