Discontinuous Precipitation in Ni-Base Superalloys During Solution Heat Treatment

  • D. Welton
  • , N. D’Souza
  • , J. Kelleher
  • , S. Gardner
  • , Z. H. Dong
  • , G. D. West
  • , Hongbiao Dong*
  • *Corresponding author for this work

Research output: Contribution to journal › Article › peer-review

Abstract

Discontinuous precipitation in single-crystal Ni-base superalloys during solution heat treatment has been studied. It is found that discontinuous precipitation occurs at temperatures approaching the solvus, where volume diffusion is dominant. Diffusion of Al ahead of the boundary leads to gamma prime precipitation and is accompanied by a loss in the driving force available for advancement of the grain boundary. The rate of gamma prime precipitation was tracked using in situ neutron diffraction during isothermal hold. Gamma prime precipitation is accompanied by super-saturation of Cr and W within the channels ahead of the interface. The driving force calculated for the initial stages of DP was [10-5 to 10-4] N/[μm2 of the grain boundary]. The results provide an insight into discontinuous precipitation during solution heat treatment of Ni-base single-crystal alloys and are useful in optimizing the heat treatment process to avoid surface defect formation.

Original languageEnglish
Pages (from-to)4298-4315
Number of pages18
JournalMetallurgical and Materials Transactions A: Physical Metallurgy and Materials Science
Volume46
Issue number9
DOIs
Publication statusPublished - 5 Sept 2015

Bibliographical note

Publisher Copyright:
© 2015, The Author(s).

ASJC Scopus subject areas

  • Condensed Matter Physics
  • Mechanics of Materials
  • Metals and Alloys

Fingerprint

Dive into the research topics of 'Discontinuous Precipitation in Ni-Base Superalloys During Solution Heat Treatment'. Together they form a unique fingerprint.

Cite this