Skip to main navigation Skip to search Skip to main content

Differential Scanning Calorimetry (DSC) and Thermodynamic Prediction of Liquid Fraction vs Temperature for Two High-Performance Alloys for Semi-Solid Processing (Al-Si-Cu-Mg (319s) and Al-Cu-Ag (201))

  • Duyao Zhang
  • , Helen V. Atkinson*
  • , Hongbiao Dong
  • , Qiang Zhu
  • *Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

Fingerprint

Dive into the research topics of 'Differential Scanning Calorimetry (DSC) and Thermodynamic Prediction of Liquid Fraction vs Temperature for Two High-Performance Alloys for Semi-Solid Processing (Al-Si-Cu-Mg (319s) and Al-Cu-Ag (201))'. Together they form a unique fingerprint.
Sort by

Keyphrases

Material Science

Engineering