Skip to main navigation Skip to search Skip to main content

A comparison study of stress corrosion crack growth rates for AA7xxx alloys as a function of bullk aqueous chloride concentrations

  • Brian Connolly
  • , MG Koul
  • , AL Moran

Research output: Contribution to journalArticle

Original languageEnglish
Pages (from-to)976-986
Number of pages11
JournalCorrosion
Volume61
Issue number10
Publication statusPublished - 1 Jan 2005